Sign In | Join Free | My chinacsw.com |
|
Brand Name : Jansincere
Model Number : MRB-003
Certification : ISO 14001, ISO9001, CE
Place of Origin : Xinmi city, Henan, China
MOQ : 1 ton
Price : $1400.00-1550.00 per ton and can be negotiable
Payment Terms : L/C, D/P, T/T, Western Union
Supply Ability : 55000 ton per year
Delivery Time : 35-40 days after received deposit
Packaging Details : Wooden pallet, plastic shrink film, paper corner protection and straps protected outside. Pallet size: 95*95cm, 100*100cm or as request.
Product Name : Sintered Brick
Product Type : Brick shape
SiO2 % : ≤18
Al2O3 % : ≥80
Bulk Density g/cm3 : ≥2.8
Apparent Porosity % : 18
Crushing Strength (MPa) : ≥90
Refractoriness Under Load(℃) : ≥1650
Thermal Shock Resistance : ≥25 times
Feature : Low Thermal Conductivity
Application : Kiln Furnace
Product Introduction:
The heavy part is made with fused mullite, fused corundum and white clay, and the light weight part is made with mullite hollow ball, cyanite, flint clay and white clay, shaped in high pressure, sintered in high temperature.
Feature:
High temperature resistance
Good abrasion resistance
Good thermal shock resistance
Good erosion resistance
Llow thermal conductivity
Technical Index:
Item | Corundum Mullite Compounding Brick | ||
Heavy | Light weight | ||
Chemical content % | Al2O3 | ≥80 | ≥35 |
SiO2 | ≤18 | 50~55 | |
Cr2O3 | / | / | |
ZrO2 | / | / | |
Fe2O3 | ≤0.8 | / | |
Apparent Porosity % | ≤18 | / | |
Crushing Strength MPa | ≥90 | ≥30 | |
RUL ℃ | ≥1650 | ≥1350 | |
Thermal Shock Resistance 1100℃ | ≥25 | / | |
Bulk Density g/cm³ | ≥2.8 | ≤2.0 | |
Thermal Conductivity ,w/m.k (600℃±25℃) | 2.0 | 1.0 | |
Refracoriness (℃) | ≥1790 | ≥1730 | |
Linear Change on Reheating(1350x3h,%) | ±0.1 | ±0.1 |
Manufacturing Process Flow:
First, qualified raw materials enter to our raw materials warehouse
Second, all materials including fine powders, aggregates, binding agent are batched according to the technical agreement.
Third, finished raw materials is shaped by 630 tons pressure machine or 2500 tons automatic hydraulic pressure machine.
Forth, green bricks is dried in the dry kilns between 40℃ and 120 ℃, and then sintering in high temperature according to the firing curve.
Last, check the quality of finished refractory bricks and qualified products are packed as request.
![]() |